4Cr13 Stainless Steel

4Cr13 Stainless Steel

4Cr13 steel (New name: 40Cr13) is a martensitic type stainless steel, which has higher hardness than 3Cr13 steel after quenching. The steel has good mechanical processing performance. After heat treatment (quenching and tempering), it has good corrosion resistance, polishing performance, high strength and wear resistance.

Have questions? GNEE sales representatives are available for live chat now

Send E-mail:info@gneestainless.com

Tel:+8615824687445

Description

Gnee Steel (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 4cr13 stainless steel in China. With abundant experience, we warmly welcome you to wholesale customized 4cr13 stainless steel from our factory. For price consultation, contact us.

 

4Cr13 Stainless Steel Introduction

4Cr13 steel (New name: 40Cr13) is a martensitic type stainless steel, which has higher hardness than 3Cr13 steel after quenching. The steel has good mechanical processing performance. After heat treatment (quenching and tempering), it has good corrosion resistance, polishing performance, high strength and wear resistance.

 

4Cr13 Steel Datasheet And Specification

The following tables list the 4Cr13 steel datasheets such as chemical composition and mechanical properties, etc.

 

Chemical Composition

4Cr13 Chemical Composition (%)

Steel Grade

C

Si (≤)

Mn (≤)

P (≤)

S (≤)

Cr

Ni (≤)

4Cr13 (40Cr13)

0.36-0.45

0.60

0.80

0.040

0.030

12.00-14.00

0.60

 

Mechanical Properties For Steel Bars

HRC hardness: ≥ 50 (Quenched and Tempered)

HBW hardness: ≤ 235 (Annealed)

Notes: For diameter or thickness ≤ 75 mm.

 

Physical Properties

Density (g/cm3): 7.75

Specific heat capacity (J/Kg·K): 460 at 0-100℃

Thermal conductivity (W/m·K):

28.1 at 100℃

28.9 at 500℃

Coefficients of linear thermal expansion (10-6/K):

10.5 (0-100℃)

12.0 (0-500℃)

Electrical Resistivity (μΩ·m): 0.59 at 20℃

Longitudinal modulus of elasticity (kN/mm2): 215 at 20℃

 

Typical Heat Treatment

Annealing: 800 – 900 ℃ (Slow cooling)

Quenching: 1050 – 1100 ℃ (Oil cooling)

Tempering: 200 – 300 ℃ (Air cooling)

 

Forging

Oil quenching cold work die steel has some crack sensitivity. It should not be heated quickly when forging heating. It’s better to preheat at 650-750 °C. The forging heating temperature is 1130-1150 °C, and the final forging temperature should be greater than 800-850 °C. The upper limit temperature is taken when the ingot is forged, and the lower limit temperature is taken when the billet is forged.

 

Applications

Stainless steel 4Cr13 is suitable for manufacturing plastic molds, transparent plastic products moulds, etc. which are subjected to high load, high wear resistance and corrosive medium.

Also used in the manufacture of hot oil pumps, tools, valve seats, valves, nozzles, measuring tools, medical equipment, springs, etc.

Stainless Steel 420 Sheet, For Industry

Hot Tags: 4cr13 stainless steel, China 4cr13 stainless steel manufacturers, factory, 410 420 440A Stainless Steel Plate 6mm, 15 5PH STAINLESS STEEL PLATE, stainless steel for special orders, stainless steel plate delivery terms, stainless steel plate price stability, stainless steel plate price trend