Home - Knowledge - Details

304 stainless steel will rust for those reasons?

Rusting of 304 stainless steel materials may occur for several reasons:


Chlorine ions
Chlorine ions are widely available, such as table salt/sweat stains/seawater/sea breeze/soil and so on. Stainless steel in the presence of chloride ions in the environment, corrosion is very fast, even more than ordinary mild steel. Therefore, the use of stainless steel environment requirements, and the need for frequent wiping, remove dust, keep clean and dry. The United States has an example: an enterprise with an oak container containing a solution containing chlorine ions, the container has been used for nearly 100 years, the last century, the nineties plan to replace the oak material is not modern enough to use stainless steel to replace the 16 days after the container leaked due to corrosion.

44e68b14a88b641d5dd0a902299cf0a


Solid solution treatment
Alloying elements are not dissolved into the matrix, resulting in low alloy content of the matrix organisation, poor corrosion resistance.
Intergranular corrosion
This material does not contain titanium and niobium has a tendency to intergranular corrosion. Intergranular corrosion can be reduced by adding titanium and niobium, together with stabilisation treatment. In the air or chemical corrosion medium can resist corrosion of a high-alloy steel, stainless steel is a beautiful surface and good corrosion resistance, do not have to go through the colour plating and other surface treatments, but to play the inherent surface properties of stainless steel, used in a variety of aspects of the steel, usually called stainless steel. The representative performance of 13 chromium steel, 18-8 chromium-nickel steel and other high-alloy steel. From the metallographic point of view, because the stainless steel contains chromium and the surface of the formation of a very thin film of chromium, this film is separated from the steel invasion of oxygen to play a role in corrosion resistance. In order to maintain the corrosion resistance inherent in stainless steel, steel must contain more than 12% chromium. It is used where welding is required. The lower carbon content minimises the precipitation of carbides in the heat-affected zone close to the weld, which can lead to intergranular corrosion (weld erosion) of stainless steel in some environments.

9d5c958ca865b687a9846eff05f6e30


Surface trace
Surface trace phenomenon is 304 stainless steel deep processing or processing products after grinding, the product surface occurs in line or point-like concave point mark defects.
Causes: foreign matter on the surface, mould surface, scarring on the surface of the crimping pad.
Countermeasures: Remove foreign objects, scars before processing, but also through the full grinding to remove orange peel.
Orange peel phenomenon refers to the 304 stainless steel moulding products in grinding or other circumstances, the surface produces a phenomenon like orange peel shape.
Reasons: insufficient grinding, the larger the processing, the more serious the orange peel, raw material grain coarseness, heat treatment softening.
Countermeasures: grinding the deep-processed products sufficiently, choosing suitable heat treatment conditions, controlling the grain size of raw materials.

44e68b14a88b641d5dd0a902299cf0a

 