Home - Knowledge - Details

ASME SB338 UNS R50400 Titanium Condenser Tubes

What Is ASME SB338 UNS R50400?

UNS R50400 is commercially pure titanium Grade 2. ASME SB338, identical to ASTM B338, covers seamless and welded titanium tubes for condensers and heat exchangers. Grade 2 is the workhorse of the titanium family: it combines the corrosion resistance of pure titanium with enough strength - 345 MPa minimum tensile - for pressure service, while remaining easy to form and weld. Grade 2H, the higher-strength variant with 400 MPa minimum tensile, is covered by the same specification and is often preferred for thicker-wall exchanger tubing.

Titanium tubes are specified where stainless steels fail: seawater and brine coolers, chlorine-containing process streams, and equipment exposed to wet chlorides, oxidizing acids and marine atmospheres. In power-plant condensers with seawater cooling, Grade 2 tubes routinely outlast the plant life.

ASME SB338 UNS R50400 Titanium Condenser Tubes
ASME SB338 UNS R50400 Titanium Condenser Tubes
ASME SB338 UNS R50400 Titanium PMI
ASME SB338 UNS R50400 Titanium PMI

ASME SB338 UNS R50400 Chemical Composition

Element Requirement (wt%) Note
Carbon 0.08 max interstitial purity control
Oxygen 0.25 max primary strength contributor
Nitrogen 0.03 max prevents embrittlement
Hydrogen 0.015 max avoids hydride formation
Iron 0.30 max main impurity
Other elements, each 0.10 max -
Other elements, total 0.40 max residual elements

Oxygen and iron are the strength-controlling interstitials. The limits above keep Grade 2 ductile enough for cold bending into U-tubes while holding the 345 MPa minimum tensile.

 

ASME SB338 UNS R50400 Mechanical Properties (Grade 2 / Grade 2H)

Property Grade 2 Grade 2H
Tensile strength, min 345 MPa (50 ksi) 400 MPa (58 ksi)
Yield strength, min 275 MPa (40 ksi) 275 MPa (40 ksi)
Yield strength, max 450 MPa (65 ksi) 450 MPa (65 ksi)
Elongation in 2 in., min 20% 20%

Both grades weld and form identically; the higher minimum tensile of 2H simply reduces scatter on the strong side of the material population. Flattening, flaring and hardness tests are standard acceptance checks per B338/SB338.

 

Design Values That Matter in Condensers

Corrosion: essentially immune to chloride pitting, crevice corrosion and stress corrosion cracking in seawater and brackish water - the reason titanium replaced copper-nickel and 316L in many coastal condensers.

Thermal conductivity: about 16-21 W/(m·K), lower than copper alloys, so tube walls are kept thin (0.4-0.7 mm typical) to keep overall heat transfer competitive.

Strength-to-weight: density 4.5 g/cm³, roughly 60% of steel, simplifying bundle handling and support design.

Fouling: the smooth, inert oxide surface resists biofouling and scale buildup, extending cleaning intervals.

System Designation Standard
ASTM/ASME Grade 2 (UNS R50400) ASTM B338 / ASME SB338
ISO Grade 2 ISO 5832-2 (implants); ISO 15156-3 (oil and gas)
EN Ti 1 EN 10216-5 / EN 10088-1
JIS Class 2; tube TP35C JIS H 4600 / JIS H 4630
GB TA2 GB/T 3625 (heat exchanger tubes)

 

Procurement Points and Equivalents

Specify the product form - seamless or welded; SB338 covers both, with welded tube subject to the same mechanical and pressure tests as seamless.

For U-bend bundles, state bend radius and tolerance on the drawing; B338/SB338 tubes are routinely cold bent, but the flattening test on the bend must be defined.

Require a material certificate with heat-number traceability (EN 10204 type 3.1 or equivalent), plus hydrostatic and eddy-current or ultrasonic testing where service demands it.

Agree surface finish: pickled or mechanically polished. Embedded iron from handling causes local corrosion on titanium, so cleanliness rules matter.

For seawater service, confirm chloride level and temperature with the exchanger designer; titanium removes the corrosion constraint, but galvanic design and flow velocity still need review.

 

FAQ

What is the difference between Grade 2 and Grade 2H titanium?

Only the minimum tensile strength: 345 MPa for Grade 2 versus 400 MPa for Grade 2H under ASTM B338. Composition and fabricability are the same, so 2H suits designs that need the extra strength margin.

 

Why is titanium used in seawater condensers?

It is effectively immune to chloride pitting, crevice corrosion and stress corrosion cracking in seawater, which 316L cannot claim in warm seawater. Tubes typically last the full plant life.

 

Is titanium Grade 2 expensive compared with stainless steel?

On material price per tonne, yes, but life-cycle cost in corrosive service is lower: no corrosion allowance, thin walls, long service life and less downtime for retubing.

 

Can Grade 2 titanium tubes be welded to tube sheets?

Yes, by TIG welding under inert-gas shielding. Cleanliness is critical: iron contamination must be removed by pickling before welding or service.

 

What is TA2 in the Chinese system?

TA2 is the GB/T 3625 designation of commercially pure titanium Grade 2 for heat exchanger and condenser tubes, with the same composition limits as UNS R50400.