ASTM A269 Seamless Stainless Steel Tubing is used for low temperature and high temperature services. These pipes could be made from austenitic steel types under electric resistant weld, electric fusion weld or seamless cold drawing mechanisms. The SA269 Tubing can also have different finishes and can be heat treated.

 

What is A269 TP316 material?

ASTM A269 Tp316 stainless steel pipe is a seamless, welded austenitic steel with a nominal wall thickness of 316 austenitic stainless steel. Composed of 16% chromium, 10% nickel, and 2% molybdenum, ASTM A269 Tp316 pipe is available in seamless, welded, and electric resistance welded (ERW) constructions. SA269 Gr 316 pipe is widely used in various pressure vessel grades. It is exceptionally strong and protects the pipe from pitting and crevice corrosion caused by stress-inducing devices.

 

A269 Grade TP316 Cold Drawn Seamless Tube HS Code

HS CODE

73044100

 

 

Equivalent material of A269 Tp316 Stainless Steel Tube

GRADE Unified Numbering System EURONORM OLD BRITISH SWEDISH
SS
Japanese Industrial Standards
NO NAME British Standards European Standards
316 S31600 1.4401 X5CrNiMo17-12-2 316S31 58H, 58J 2347 SUS 316

 

ASME SA269 Tp 316 Tubing Chemical Composition

Grade   Manganese Sulfur Silicon Carbon Phosphorus Chromium Molybdenum Nickel Nitrogen
Tp316 Minimum         0 16.0 2.00 10.0  
maximum 2.0 0.03 0.75 0.08 0.045 18.0 3.00 14.0 0.10

 

ASTM A269 Gr Tp316 Tube Mechanical Properties

Grade Tensile Str
(Mpa) Min
Elongation
Minimum
Yield Str
(Mpa) Min
Hardness
Rockwell B (Hr B) Max Brinell (Hb) Max
Tp316 515 40 205 95 217

 

ASME SA269 Tp 316 Seamless Tubing Physical Properties

Grade Density
(Kg/m3)
Elastic Modulus
(Gpa)
Thermal Conductivity
(W/m.k)
Mean Co-eff Of Thermal Expansion (μm/m/°c) Specific Heat 0-100°c
(J/kg.k)
Elec Resistivity
(Nω.m)
AT 100°C AT 500°C 0-100°C 0-315°C 0-538°C
316 8000 193 16.3 21.5 15.9 16.2 17.5 500 74

 

SA269 Grade TP316 Welded Tube Corrosion Resistance

Corrosion Resistance Temperature Range (°C)
Pitting and Crevice Corrosion Resistance -196°C - 60°C
Corrosion Resistance -196°C - 870°C

 

Is ASTM A269 TP316 Schedule 40 or Schedule 80 Stronger?

SCH 80 SA 269 TP 316 Seamless Tubes have greater wall thickness than SCH 40 ones. This means that sch 80 is able to withstand higher pressure ratings and has greater strength. Thus, sch 40 tubes are ideal for low pressure applications. Whereas, sch 80 tubes are used for industrial and chemical applications.

 

SA 269 Gr 316 Heat Exchanger Tubes Test Method

Flattening Test

One flattening test shall be made on specimens from each end of one finished tube, not the one used for the flaring test, from each lot.

Flaring Test

One flaring test shall be made on specimens from each end of one finished tube, not the one used for the flattening test, from each lot.

Hydrostatic or Nondestructive Testing

Each pipe shall be subjected to the nondestructive electric test or the hydrostatic test, the type of test to be used shall be at the option of the manufacturer, unless otherwise specified in the purchase order.

 

If you have a project need for ASTM A269 TP316 stainless steel pipe, we welcome your order. GNEE has a large inventory of popular products for you to choose from. We offer a variety of practical product forms, including seamless and welded. For detailed chemical composition and free samples, please contact our factory today. We offer competitive pricing and excellent service.

Click to download ASTM A269 material list