1.4310 Stainless Steel: Composition, Properties & Uses
Leave a message
What Is 1.4310 Stainless Steel?
1.4310, designated X10CrNi18-8 in EN 10088, is a high-carbon austenitic stainless steel in the 301 family. Its defining characteristic is rapid work hardening: cold rolling or cold drawing raises tensile strength from about 520 MPa in the annealed condition to 730-900 MPa or beyond at modest deformation, without losing the ductility needed for springs and formed parts. The grade is therefore the standard choice for stainless springs, clips, fasteners, woven wire and conveyor belting.
The material is delivered to EN 10088-2 (strip, sheet, plate) or EN 10088-3 (bar), usually in the solution-annealed condition, so that the customer's cold-working step produces the final strength.
Chemical Composition
| Element | 1.4310 X10CrNi18-8 (EN 10088) | AISI 301 | 12Cr17Ni7 (GB/T 3280) |
|---|---|---|---|
| Carbon | 0.05-0.15 | 0.15 max | 0.12 max |
| Silicon | 1.00 max | 1.00 max | 1.00 max |
| Manganese | 2.00 max | 2.00 max | 2.00 max |
| Phosphorus | 0.045 max | 0.045 max | 0.045 max |
| Sulfur | 0.015 max | 0.030 max | 0.030 max |
| Chromium | 16.0-19.0 | 16.0-18.0 | 16.0-18.0 |
| Nickel | 6.0-9.5 | 6.0-8.0 | 6.0-8.0 |
| Nitrogen | 0.11 max | 0.10 max | - |
The 0.05-0.15% carbon range is the key difference from 304: more carbon means more martensite forms during cold work, which is exactly what produces spring hardness. The trade-off is that heavy-section welds are prone to sensitization, so the grade is best used in thin sections or where welding is minimal.
Physical and Mechanical Properties
| Property | Value | Condition |
|---|---|---|
| Density | 7.9 g/cm³ | 20°C |
| Melting range | 1380-1420°C | - |
| Thermal conductivity | 15 W/(m·K) | 20°C |
| Mean CTE (20-100°C) | 16.0 x 10⁻⁼ 1/K | - |
| Electrical resistivity | 0.73 μΩ·m | 20°C |
| Elastic modulus | 200 GPa | 20°C |
| Tensile strength | ≥520 MPa (annealed); 730-900 MPa (cold-worked) | as specified |
| Yield strength Rp0.2 | ≥205 MPa (annealed); 260-570 MPa (cold-worked) | as specified |
| Elongation | ≥40% (annealed); 14-45% (cold-worked) | as specified |
| Hardness | 200-270 HB (annealed) | as specified |
For spring strip, strength is ordered by temper class: EN 10151 classes C850, C1400 and C1900 guarantee minimum tensile strengths of 850, 1400 and 1900 MPa respectively. Fatigue strength at 10&sup7; cycles is typically 240-330 MPa in hardened tempers.
Typical Applications
Springs: valve springs, clip springs, leaf-type contact springs, spring washers
Fasteners and pins in instruments and appliances
Woven wire and conveyor belting in food and packaging lines
Wiper blades, zipper strip, cable reinforcement, hose clamps
Structural springs and trim parts in rail and automotive builds
Selection and Fabrication Points
Order by temper class (C850, C1400 or C1900 per EN 10151) so delivered hardness matches the spring design.
Expect slight magnetism after cold work: strain-induced martensite is ferromagnetic, which is normal for this grade.
For welded parts, keep to thin sections and light duty; the high carbon content makes heavy welds prone to sensitization.
Stress-relieve formed springs at 350-450°C to remove residual stress without losing work-hardened strength.
Frequently Asked Questions
Q: What is the difference between 1.4310 and 1.4301 (304)?
Carbon content: 1.4310 contains 0.05-0.15% C versus about 0.07% max for 1.4301. The higher carbon enables the strain hardening that gives 1.4310 its spring strength; it also reduces weldability of heavy sections.
Q: Is 1.4310 the same as AISI 301?
Close but not identical: 1.4310 allows 16.0-19.0% Cr and 6.0-9.5% Ni, while AISI 301 specifies 16.0-18.0% Cr and 6.0-8.0% Ni, with a lower sulfur limit in the EN version. For spring applications they are treated as equivalents.
Q: Why does 1.4310 become magnetic when cold worked?
Cold deformation transforms part of the austenite into strain-induced martensite, which is ferromagnetic. The effect is intentional: it is the same transformation that raises strength and hardness.
Q: Can 1.4310 be used for springs in corrosive environments?
In mild atmospheric and food-contact conditions, yes, with the surface kept clean. In chloride or marine environments, consider a 316 spring temper where chloride resistance matters more than maximum strength.
Q: What does the EN 10151 temper class C850 mean?
It is the minimum tensile strength class of cold-rolled spring strip: C850 guarantees at least 850 MPa in the delivered temper, with correspondingly higher values for C1400 and C1900.
Q: What is the chemical composition of 1.4310?
1.4310 (X10CrNi18-8) contains 0.05-0.15% carbon, 16.0-19.0% chromium, 6.0-9.5% nickel, 1.00% max silicon, 2.00% max manganese, 0.045% max phosphorus, 0.015% max sulfur and 0.11% max nitrogen. The higher carbon range is what drives the strain-induced martensite that gives the grade its spring hardness.