ASTM A789 UNS S31803 Stainless Steel Heat Exchanger Tubes
Specification:ASTM A789, ASME SA789
Grades:UNS S31803, S32205
Manufacturing Method:Cold Rolling, Cold Drawn
Outside Diameter:6 – 610 mm
Wall Thickness:0.5 – 30 mm, Average Wall Or Minimum Wall
Length:Specific or Rando, standard 6000 mm length
Condition:Annealing Pickling, Beight Annealing
Form::Round, Coiled Tubing
Application:Heat Exchanger, Boiler, Water, High Pressure, Ornamental Purpose
Send E-mail:info@gneestainless.com
Tel:+8615824687445
Description
Gnee Steel (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ASTM A789 UNS S31803 Stainless Steel Heat Exchanger Tubes in China. With abundant experience, we warmly welcome you to wholesale customized ASTM A789 UNS S31803 Stainless Steel Heat Exchanger Tubes from our factory. For price consultation, contact us.
If you are looking for cost-effective duplex stainless steel heat exchanger tubes suitable for chloride-rich petrochemical, seawater cooling, and energy projects, ASTM A789 UNS S31803 stainless steel tubes feature a balanced austenitic-ferritic duplex microstructure. With a minimum yield strength of 450 MPa and tensile strength up to 620 MPa-nearly twice that of traditional 316L austenitic stainless steel tubes-they allow for thinner wall designs, reducing equipment weight and capital expenditures without sacrificing safety margins.
Featuring a PREN ≥ 32, ASTM A789 UNS S31803 duplex tubes offer excellent resistance to chloride-induced pitting, crevice corrosion, and stress corrosion cracking. With a critical pitting temperature (CPT) ≥ 40°C, their service life in brackish water and acidic working conditions is 2–3 times that of 316L stainless steel. Suitable for condensers, process heat exchangers, and utility cooling loops, they have a minimum elongation of 25%, ensuring reliable cold forming and tube sheet expansion performance.
GNEE Stainless Steel has successfully completed over 30 energy and petrochemical project cases, with product exports reaching more than 60 countries and acceptance of third-party certifications from SGS, BV, TÜV, and others. We provide ASTM A789 UNS S31803 heat exchanger tubes with outer diameters from 6mm to 114.3mm, wall thicknesses from 1.0 to 8.0mm, and customizable lengths (random or fixed), with surface finish options including bright annealing or pickling, as well as ready-to-install U-bend tubes. Every batch comes with an EN 10204 3.1 Mill Test Certificate, complete heat number traceability, and mandatory PMI material verification, hydrostatic testing, and eddy current testing to ensure tube integrity.



Duplex Steel UNS S31803 Pipes Specification
ASTM A789 UNS S31803 tube Chemical & Mechanical Properties
| C | Mn | P | S | Si | Cr | Ni | Mo | N |
| ≤ 0.030% | ≤ 2.00% | ≤ 0.030% | ≤ 0.020% | ≤ 1.00% | 21.0 - 23.0% | 4.5 - 6.5% | 2.5 - 3.5% | 0.08 - 0.20% |
Physical Properties of A789 UNS S31803 welded tube
| Grade | Density (kg/meter3) | Elastic Modulus (GPa) | Mean Co-efficent of Thermal Expansion (μm/meter/°C) | Specific Heat 0-100°C ( J/kg.K) | Thermal Conductivity (W/m.K) | Electrical Resistivity (nΩ.m) | |||
| 0 to 100°C | 0 to 315°C | 0 to 538°C | at 100°C | at 500°C | |||||
| UNS S31803 | 782 | 190 | 13.7 | 14.2 | - | 418 | 19 | - | 850 |
Mechanical Properties of SA 789 UNS S31803 ERW Tube
| Tensile Strength,min. | Yield Strength,min. | Elongation,min. | Hardness Brinell, max |
|---|---|---|---|
| Mpa | Mpa | % | HB |
| 620 | 450 | 25 | 290 |
ASTM A789 Stainless Steel Tubing Tolerances
| Outside Diameter, In. [Mm] |
OD Tolerance, In. [Mm] |
Average Wall In Wall Thickness,% |
Minimum Wall In Wall Thickness, %, Over |
Minimum Wall In Wall Thickness, %, Under |
Cut Length, In. [Mm], Over |
Cut Length, In. [Mm], Under |
Thin Walled Tubes |
|---|---|---|---|---|---|---|---|
| Up To 1⁄2 [12.7], Excl | ±0.005 [0.13] | ±15 | 30 | 0 | 1⁄8 [3] | 0 | … |
| 1⁄2 To 11⁄2 [12.7 To 38.1], Excl | ±0.005 [0.13] | ±10 | 20 | 0 | 1⁄8 [3] | 0 | Less Than 0.065 In. [1.6 Mm] Specified |
| 11⁄2 To 31⁄2 [38.1 To 88.9], Excl | ±0.010 [0.25] | ±10 | 20 | 0 | 3⁄16 [5] | 0 | Less Than 0.095 In. [2.4 Mm] Specified |
| 31⁄2 To 51⁄2 [88.9 To 139.7], Excl | ±0.015 [0.38] | ±10 | 20 | 0 | 3⁄16 [5] | 0 | Less Than 0.150 In. [3.8 Mm] Specified |
| 51⁄2 To 8 [139.7 To 203.2], Incl | ±0.030 [0.76] | ±10 | 20 | 0 | 3⁄16 [5] | 0 | Less Than 0.150 In. [3.8 Mm] Specified |
What is the difference between S31803 and S32205?
S32205 is an "enhanced" version of S31803. To improve corrosion resistance, S32205 has higher minimum requirements for the content of chromium, molybdenum, and nitrogen (N). Most ASTM A789 pipes on the market today are dual certified. They are interchangeable as long as the chemical composition meets the requirements of both grades. S32205 generally has better resistance to pitting corrosion.
What is the maximum service temperature for S31803?
Recommended upper limit: Approximately 300°C (572°F). Prolonged exposure above 300°C (especially the 475°C embrittlement zone) will cause "475°C embrittlement" in duplex steel, leading to a significant decrease in toughness and corrosion resistance. Therefore, it is not suitable for extremely high-temperature applications.
ASTM A789 S31803 Tubes Application:
Oil & Gas: Offshore platforms, downhole tubing, piping for corrosive wells.
Chemical & Petrochemical Processing: Heat exchangers, pressure vessels, process piping.
Power Generation: Feedwater heaters, condenser tubes.
Desalination & Marine: Seawater handling equipment, reverse osmosis plants.
Pulp & Paper Industry: Digester and bleach plant equipment.
If you are planning a project or making a purchase, please let me know:
Do you require seamless or welded pipes?
What are the required dimensions (outside diameter and wall thickness) and quantities?
I can assist you in determining the relevant testing standards or matching specifications.
Quality Control
| Inspection Category | Test Item | Purpose / Standard Requirement |
|---|---|---|
| Chemical Composition | Chemical Analysis | Verify that Cr, Ni, Mo, N and other alloying elements comply with the requirements for UNS S31803/S32205 dual-grade designation. |
| Hardness | Hardness Test | Ensure hardness is within the applicable standard range, typically ≤31 HRC or ≤293 HBW for Duplex 2205. |
| Fabrication Tests | Flattening & Flaring Tests | Verify tube ductility and integrity during flattening, flaring and heat-exchanger tube expansion, ensuring no cracking occurs. |
| Metallographic Examination | Ferrite Content | Determine the ferrite/austenite phase balance. A project-specific range such as 35–65% ferrite may be specified and verified by metallographic examination, e.g. ASTM E562. |
| Microstructural Examination | Sigma Phase Check | Check for harmful sigma phase and other detrimental intermetallic phases, with ASTM A923 testing applied when specified. |
| Non-Destructive Testing (NDT) | Eddy Current Testing (ET) | 100% Eddy Current Testing can be performed to detect surface and near-surface discontinuities such as cracks, pinholes and other tube-wall defects. |






Standard Export Packaging
Plastic Caps: Secure plastic caps are fitted to both ends of each tube to prevent the ingress of dust and moisture.
Surface Finish: The surface is typically pickled and passivated; a thin layer of protective oil can be applied upon request.
Reinforced Wooden Cases (Recommended): Reinforced wooden cases are the preferred choice for export. Internal dividers are included to ensure the tubes do not shift or bend during transport.


FAQ
1. How do you ensure the ferrite content remains between 40% and 55%?
For Duplex 2205 steel pipes, we conduct a final metallographic examination; ferrite content can be verified using ASTM E562, ASTM E1245, or equivalent certified metallographic/magnetic testing methods, in accordance with project specifications. For critical heat exchanger applications, ferrite content testing can be incorporated into the Inspection and Test Plan (ITP) and reported in the Material Test Certificate (MTC) or a supplementary inspection report.
2. Can you provide a test report for ASTM G48 Method A (pitting corrosion test)?
Yes, we can provide ASTM G48 Method A testing if required by the customer or the project. This test evaluates the pitting and crevice corrosion resistance of stainless steels and related alloys in ferric chloride solution. The report includes test temperature, exposure time, specimen details, and corrosion assessment results.
3. Is post-bending heat treatment performed on the bent sections of U-bend pipes?
Yes, heat treatment can be performed in accordance with applicable standards and customer requirements. Following U-bend forming, the pipes may undergo solution annealing or stress-relief treatment, depending on the steel grade, bend radius, wall thickness, and project specifications.
4. Can the MTC (Material Test Certificate) support dual-grade designation for S31803/S32205?
Yes, though this depends on the actual chemical composition and applicable specification requirements. When the material meets the requirements for both UNS S31803 and UNS S32205, and the procurement specification permits dual-grade designation, the MTC can identify the material as UNS S31803/S32205 Duplex 2205. The certificate includes the heat number, chemical composition, tensile strength, yield strength, elongation, hardness, heat treatment condition, and test results to ensure full material traceability.
Hot Tags: ASTM A789 UNS S31803 Stainless Steel Heat Exchanger Tubes, China ASTM A789 UNS S31803 Stainless Steel Heat Exchanger Tubes manufacturers, factory, 304 Stainless Steel Welded Pipe, Stainless Steel Welded Pipe, 316L Stainless Steel Welded Pipe, ASTM A269 Welded Austenitic Stainless Steel Tubing, ss 304 welded pipe, ss 316L Welded pipe
Send Inquiry
You Might Also Like