1.4541 vs. 1.4878 Stainless Steel: Composition
Leave a message
What is 1.4541 SS equivalent to?
The material AISI 321 is an austenitic stainless steel that is also known under the designations 1.4541, Alloy 321, BS 321S31, BS 321S51 and X6CrNiTi18-10. The material is a V2A steel that has been stabilised by the addition of titanium and is characterised by good corrosion resistance (PREN value 17.0 to 19.0).
What is 1.4878 steel number?
Material No. AISI 321 H / 1.4878 is an austenitic, heat-resistant stainless steel. It offers moderate resistance to carburized gases and low resistance to oxidized and reduced sulfuric gases. It can be processed into a variety of practical product forms, including sheet, coil, tube, bar, and wire.
1.4541 vs. 1.4878 Stainless Steel: Composition
The main difference is the higher carbon content in 1.4878 (0.04-0.10%) compared to 1.4541 (≤ 0.08% max in some standards, but can vary), which is sometimes listed with a lower carbon content.
1.4541 vs. 1.4878 Stainless Steel Chemical Composition (EN standard ranges, wt.%)
| Element | 1.4541 (AISI 321) | 1.4878 (AISI 321H) |
|---|---|---|
| C (Carbon) | ≤ 0.08% | 0.04 – 0.10% |
| Si (Silicon) | ≤ 1.00% | ≤ 1.00% |
| Mn (Manganese) | ≤ 2.00% | ≤ 2.00% |
| P (Phosphorus) | ≤ 0.045% | ≤ 0.045% |
| S (Sulfur) | ≤ 0.015% | ≤ 0.015% |
| Cr (Chromium) | 17.0 – 19.0% | 17.0 – 19.0% |
| Ni (Nickel) | 9.0 – 12.0% | 9.0 – 12.0% |
| Ti (Titanium) | ≥ 5 × C, ≤ 0.70% | ≥ 4 × C, ≤ 0.70% |
1.4541 vs. 1.4878 Stainless Steel Mechanical Properties (at room temperature)
| Property | 1.4541 (AISI 321) | 1.4878 (AISI 321H) |
|---|---|---|
| Tensile Strength (Rm) | 500 – 700 MPa | 520 – 750 MPa |
| Yield Strength (Rp0.2) | ≥ 200 MPa | ≥ 210 MPa |
| Elongation (A5) | ≥ 40% | ≥ 35% |
| Hardness (HB) | ≤ 215 | ≤ 217 |
| Operating Temperature | Up to ~870 °C | Up to ~950 °C (better creep resistance) |
1.4541 vs. 1.4878 Stainless Steel :Corrosion Resistance
1.4541 and 1.4878 offer similar, good corrosion resistance in neutral environments and are resistant to intergranular corrosion, but both are susceptible to pitting corrosion in warm chloride-rich environments like sea air or seawater. Material 1.4878 is a heat-resistant version of 1.4541, with slightly higher carbon and titanium content, allowing it to be used at higher temperatures (up to 850°C) compared to 1.4541.
1.4541 vs. 1.4878 Stainless Steel :Heat Resistance
While 1.4541 and 1.4878 share similar heat resistance, with both being used in temperatures up to 850-900°C in air, 1.4878 (AISI 321H) has a higher maximum operating temperature in a neutral environment, reaching up to 850°C compared to 1.4541's (AISI 321) 870°C for intermittent service and 925°C for continuous service but is better suited for applications up to 850°C.
What is 1.4541 vs 1.4301 material?
1.4541 is titanium-stabilized, making it more resistant to carbide precipitation during welding and high-temperature service, whereas 1.4301 lacks this stabilization and may become sensitive to corrosion when exposed to temperatures above 425°C.

who choose us?
If you have a project need for 321 stainless steel plate, we welcome your order. GNEE has a large inventory of popular products for you to choose from. We offer a variety of practical product forms, including hot-rolled and cold-rolled. For detailed chemical composition and free samples, please contact our factory today. We offer competitive pricing and excellent service. Email: info@gneestainless.com