uns s31083 vs. uns s32205 Duplex stianless steel
Leave a message
What Is UNS S31803?
UNS S31803 is a duplex stainless steel that combines the advantages of both austenitic and ferritic microstructures. It offers excellent strength, stress corrosion cracking resistance, and pitting corrosion resistance in chloride-rich environments.
What Is UNS S32205 Material?
UNS S32205 is an improved version of S31803, with tighter control over the nitrogen content and a more refined chemical composition to ensure a better phase balance between austenite and ferrite.
Is S31803 the Same as S32205?
Yes,Both S31803 and S32205 belong to the 2205 duplex stainless steel family. S31803 was the original designation, but as metallurgy improved, S32205 was introduced to provide more reliable phase stability and corrosion resistance.In most applications today, S32205 is used as the standard for 2205, and many suppliers consider S31803 and S32205 to be interchangeable, though technically, S32205 has stricter limits and better corrosion performance.
S31803 vs. S32205: Chemical Composition Comparison
| Element | S31803 (%) | S32205 (%) |
|---|---|---|
| Chromium (Cr) | 21.0 – 23.0 | 22.0 – 23.0 |
| Nickel (Ni) | 4.5 – 6.5 | 4.5 – 6.5 |
| Molybdenum (Mo) | 2.5 – 3.5 | 3.0 – 3.5 |
| Nitrogen (N) | 0.08 – 0.20 | 0.14 – 0.20 (tighter) |
| Carbon (C) | ≤ 0.030 | ≤ 0.030 |
| Manganese (Mn) | ≤ 2.0 | ≤ 2.0 |
S31803 vs. S32205 stainless steel:Mechanical Properties
| Property | S31803 / S32205 (Typical) |
|---|---|
| Yield Strength | ≥ 450 MPa |
| Tensile Strength | ≥ 620 MPa |
| Elongation | ≥ 25% |
| Hardness (HBW) | ≤ 290 |
Difference Between S31803 and S32205
Heat Treatment of S31803 and S32205
After cold working or welding, these materials should undergo solution annealing at temperatures between 1040–1100°C, followed by rapid cooling via water quenching or forced air cooling to retain their duplex microstructure and mechanical properties.
Weldability of S31803 and S32205
Both S31803 and S32205 duplex stainless steels are readily weldable using processes such as TIG welding, SMAW (stick welding), and plasma arc welding. It is recommended to use nitrogen-enhanced filler metals (e.g., ER2209) with a nitrogen content of at least 0.12%.
1.Preheating is not required, but interpass temperature should be kept below 100°C to prevent the formation of sigma phase and other intermetallic compounds.
2.Post-weld PT (penetrant testing) is advised to verify weld quality.
Machinability of S31803 and S32205
S31803 and S32205 duplex stainless steels exhibit hot strength comparable to Type 430 stainless steel in the high-temperature range of 950–1150°C. However, below 900°C, their yield strength increases sharply, making them significantly more difficult to process.
During cold working, special attention is required. Their yield strength is approximately 50% higher than that of Type 304 stainless steel, while elongation is about 30% lower. It is recommended to use low cutting speeds combined with high-performance cutting tools, such as carbide-coated inserts, to reduce the risk of cracking caused by work hardening.
Looking for Duplex 2205 Stainless Steel?
GNEE Stainless Steel supplies high-quality S32205 / S31803 duplex stainless steel in plates, pipes, tubes, flanges, and custom-machined parts.
✔ Certified to ASTM A240 / A790 / EN 10088
✔ Third-party tested chemical and mechanical properties
✔ In-stock or custom-cut formats available
✔ Technical support for material selection and processing
📩 Contact us now for a quote, datasheet, or sample.