X12Cr13 /1.4006 /410 Martensitic stainless steel
Leave a message
This guide answers common buyer questions about X12Cr13 / 1.4006 / 410 stainless steel, including its chemical composition, equivalent grades, heat treatment behavior, and typical applications.
What Is X12Cr13 / 1.4006 / 410 Stainless Steel?
This steel belongs to the martensitic family, which means it can be hardened by heat treatment-unlike austenitic types like 304 or 316.
| Designation | Standard | Description |
|---|---|---|
| X12Cr13 | EN 10088-1 | Steel with 12% Cr, martensitic structure |
| 1.4006 | EN | Werkstoffnummer for X12Cr13 |
| AISI 410 | ASTM | Equivalent American grade |
1.4006 / 410 stainless steel Chemical Composition (Typical, wt%)
| Element | Content (%) |
|---|---|
| Carbon (C) | 0.08 – 0.15 |
| Chromium (Cr) | 11.5 – 13.5 |
| Manganese (Mn) | ≤ 1.0 |
| Silicon (Si) | ≤ 1.0 |
| Phosphorus (P) | ≤ 0.04 |
| Sulfur (S) | ≤ 0.03 |
| Iron (Fe) | Balance |
1.4006 / 410 stainless steel Mechanical Properties (After Quenching & Tempering)
| Property | Value (Typical) |
|---|---|
| Tensile Strength | 500 – 750 MPa (annealed), up to 1000 MPa (hardened) |
| Yield Strength | ≥ 300 MPa |
| Hardness (HBW) | ~200–300 (annealed), up to 400+ (hardened) |
| Elongation (A5) | 15 – 20% |
| Density | ~7.75 g/cm³ |
| Magnetic | Yes |
1.4006 / 410 stainless steel Heat Treatment
X12Cr13 / 1.4006 is air or oil hardenable, and its properties depend heavily on heat treatment:
Annealing: 800–850°C followed by slow cooling (soft structure)
Hardening: 980–1050°C followed by rapid cooling (martensitic structure)
Tempering: 200–600°C to reduce brittleness and adjust hardness
⚠️ Temper at temperatures above 400°C to avoid temper embrittlement.
What is the equivalent treatment for 1.4006/410 Stainless Steel?
| Standard | Equivalent Grade |
|---|---|
| ASTM/SAE | AISI 410, UNS S41000 |
| EN | X12Cr13, 1.4006 |
| JIS | SUS410 |
| GB | 1Cr13 |
| ISO | X12Cr13 |
What Is The Difference Between SUS410 And 304 Stainless Steel?
SUS410 (martensitic Cr13 series, carbon ≤0.15%, nickel-free) can be hardened and strengthened, with high strength (tensile strength ≥440MPa) but weak corrosion resistance, and is suitable for tool bearings.
304 (austenitic 18Cr-8Ni, carbon ≤0.08%) has excellent corrosion resistance and plasticity (elongation ≥40%) due to its nickel content, non-magnetic and no need for heat treatment after welding, and is mostly used in food equipment and decoration.
We supply X12Cr13 / 1.4006 / AISI 410 stainless steel in multiple forms and heat-treated conditions, with full EN 10204 3.1 certification, fast delivery, and global export packaging. Ideal for machined components, hardened wear parts, and custom forging.
Form: Sheet, plate, round bar, forged parts, pipe
Thickness: 2 mm to 100 mm
Surface: Pickled, ground, rough machined
Standards: EN 10088-2, ASTM A240, A276, A479
Condition: Annealed, hardened + tempered (QT800/QT900)
📧 Email us now for a datasheet, quote, or cut-to-size service