Home - Knowledge - Details

X2CrNiN18-10 / 1.4311 / 304LN Stainless Steel: Composition, Properties and Applications

What Is X2CrNiN18-10 (1.4311 / 304LN)?

X2CrNiN18-10 is the EN designation for material number 1.4311, the nitrogen-bearing variant of 304L austenitic stainless steel. The same material is listed as AISI/ASTM 304LN (UNS S30453) in the American system, as SUS304LN in JIS, and as 00Cr19Ni10N in the GB system. Nitrogen is a strong austenite stabiliser and an interstitial strengthener, so the grade delivers a distinctly higher 0.2% proof strength than 304L while keeping the corrosion behaviour, formability and weldability of the standard 18-8 family.

In purchasing practice the grade is normally specified where a designer wants to cut wall thickness, flange mass or structural weight without moving up to a molybdenum-bearing grade such as 316L.

Chemical Composition and Governing Standards

The composition limits below are those published for UNS S30453 in ASTM A240/A240M, the reference specification for stainless steel plate, sheet and strip. European deliveries of the same grade are covered by EN 10088-2 (strip, plate and sheet), EN 10028-7 (pressure-purpose plate), EN 10216-5 (seamless pressure tube) and EN 10217-7 (welded pressure tube), all under the designation 1.4311.

Element ASTM A240/A240M 304LN (%)
C ≤ 0.030
Mn ≤ 2.00
P ≤ 0.045
S ≤ 0.030
Si ≤ 0.75
Cr 18.0 - 20.0
Ni 8.0 - 12.0
N 0.10 - 0.16

The controlled nitrogen range is the single feature that separates 304LN from 304L. A minimum of 0.10% N is enough to raise the proof strength by roughly one third, while the carbon ceiling of 0.030% keeps resistance to intergranular attack after welding comparable to that of 304L.

Mechanical Properties in the Annealed Condition

The values below are typical, informative figures for solution-annealed product. Guaranteed minima vary with product form, dimension and edition of the applicable standard.

Property Typical value
Tensile strength, Rm 550 - 750 MPa
0.2% proof strength, Rp0.2 250 - 320 MPa
Elongation, A 45 - 55%
Hardness ≤ 215 HBW
Charpy V-notch, room temperature 100 J and above

Because the nitrogen addition lifts allowable design stress, pressure equipment code cases permit thinner components than grade 304L for the same duty. The density of the grade is 7.9 g/cm3, modulus of elasticity about 200 GPa at 20 °C, and thermal conductivity about 15 W/m·K, all close to 304L.

Corrosion Behaviour

Pitting resistance equivalent is only slightly improved relative to 304L, since the grade contains no molybdenum; PRE values normally fall between 18 and 20. The material performs well in fresh water, most organic media, nitric acid service and mildly oxidising environments, but it is not a substitute for 316L or duplex grades in chloride-rich or strongly reducing conditions. In pulp, paper, food and pharmaceutical plants it is usually chosen for high-pressure or high-cycle sections where fatigue strength and stiffness matter more than pitting resistance.

Fabrication and Welding

Fabrication follows the rules used for 304L. Shearing, plasma and laser cutting, cold bending and roll forming are all performed on the same equipment. The grade work-hardens rapidly, so machining uses positive rake tooling, generous feed and continuous cutting to avoid a glazed surface layer. Welding is carried out with matching 308L filler metal classified under AWS A5.9, or with ER308L/ER308LSi for thin gauge. Heat input should be controlled, interpass temperature kept below about 150 °C, and the weld surface cleaned of oxide and iron contamination before service. Post-weld heat treatment is not required for the low-carbon grade; procedure qualification is normally performed to ASME BPVC Section IX or EN ISO 15614-1.

Frequently Asked Questions

Q: Is X2CrNiN18-10 the same as 304LN?
A: Yes. X2CrNiN18-10 with material number 1.4311 is the EN designation, and 304LN (UNS S30453) is the ASTM/AISI designation for the same nitrogen-bearing austenitic grade.

Q: How much stronger is 1.4311 than 304L?
A: The nitrogen range of 0.10-0.16% typically raises the 0.2% proof strength from about 200-210 MPa for 304L to 250-320 MPa, roughly a one-third increase, while tensile strength stays in the same general band.

Q: Can 304LN be welded without post-weld heat treatment?
A: Yes. With a carbon ceiling of 0.030% the risk of sensitisation is low, so normal practice is to weld with 308L filler and leave the joint in the as-welded condition. Solution annealing is only applied when the service environment demands it.

Q: Is 304LN resistant to chloride pitting?
A: It has slightly better pitting resistance than 304L but contains no molybdenum, so it is not suitable for hot chloride brines or seawater. For those duties a molybdenum-bearing or duplex grade is required.

Q: Which product forms are commonly ordered?
A: Cold rolled sheet and strip in 2B, BA or polished finish, hot rolled plate, seamless and welded tube, and bar for machined parts. Thicknesses and tolerances follow ASTM A240/A240M or EN 10088-2 unless another specification is stated on the order.

Q: What documentation is normally supplied with the material?
A: A mill test certificate to EN 10204 type 3.1 listing heat number, chemical analysis and mechanical test results, with optional third-party inspection or additional impact testing where the end use requires it.

Send Inquiry