Stainless Steel 1.4435 vs 1.4401 - What's the Difference?

What is the equivalent astm of 1.4401 stainless steel ?

The equivalent of European standard EN 1.4401 stainless steel is American standard AISI 316 or UNS S31600. This grade of austenitic stainless steel contains molybdenum, which provides enhanced corrosion resistance, particularly in environments with chlorides, and is also known by its chemical designation X5CrNiMo17-12-2.

 

What is the equivalent of 1.4435 stainless steel?

The equivalent of EN 1.4435 stainless steel is AISI 316L Mo or S31603, a specific grade of the 316L series with a higher molybdenum content for enhanced corrosion resistance, also sometimes referred to as X2CrNiMo18-14-3 under the EN norm. While 1.4435 is often compared to the standard 316L (1.4404), it offers improved resistance to acids and chlorides due to its elevated alloy composition.

 

 

What is the difference between 1.4435 and 1.4401 stainless steel?

 

Both 1.4435 (AISI 316L Mo ) and 1.4401 (AISI 316) are molybdenum-containing stainless steels, but the key difference lies in their carbon content. 1.4435 (AISI 316L Mo) has a lower carbon content (≤ 0.03%), making it more suitable for welding applications, as it reduces the risk of carbide precipitation and improves resistance to intergranular corrosion in the heat-affected zone. In contrast, 1.4401 (316) has a higher carbon content (≤ 0.08%) and may require post-weld heat treatment to avoid sensitization. Carbon content is a critical factor to consider in stainless steels.

 

Chemical composition

Property 1.4401 (AISI 316) 1.4435 (AISI 316L)
Chemical Composition    
Carbon (C) ≤ 0.08% ≤ 0.03%
Chromium (Cr) 16.00% - 18.00% 16.00% - 18.00%
Nickel (Ni) 10.00% - 14.00% 10.00% - 14.00%
Manganese (Mn) ≤ 2.00% ≤ 2.00%
Silicon (Si) ≤ 1.00% ≤ 1.00%
Phosphorus (P) ≤ 0.045% ≤ 0.045%
Sulfur (S) ≤ 0.030% ≤ 0.030%
Molybdenum (Mo) 2.00% - 3.00% 2.00% - 3.00%

 

Mechanical properties

Mechanical Properties

   
Tensile Strength (MPa) 520 - 700 MPa 480 - 700 MPa
Yield Strength (MPa) ≥ 240 MPa ≥ 170 MPa
Elongation (%) ≥ 40% ≥ 40%
Hardness (HRB) ≤ 90 HRB ≤ 90 HRB

 

What is the difference between 1.4404 and 1.4435?
1.4435 stainless steel is an austenitic, highly corrosion resistant material. 1.4435 material has a higher content of chromium, nickel and molybdenum. Due to the effects of these elements, it is more corrosion resistant than the 316L (1.4404) grade. 1.4435 grade is not magnetic. 1.4435 stainless steel may be a very good alternative material if the 316L grade is not sufficient.

 

What is the difference between 1.4436 and 1.4401?

The main difference is that 1.4436 has a higher molybdenum (Mo) content (2.50-3.00%) compared to 1.4401 (which has around 2-2.5% Mo), making 1.4436 a more highly alloyed grade with superior corrosion resistance, particularly against pitting and chloride-containing environments.

 

 

Products Description

 

When choosing 1.4435 and 1.4401 stainless steel for your project, you need to consider several factors, including corrosion resistance, weldability, high-temperature resistance, and cost constraints, depending on the project type and application.
If you have a project requirement for 316 1.4401 stainless steel, please feel free to place an order. GNEE has a large inventory of popular products for you to choose from. They can be processed into a variety of practical product forms, including sheet, coil, tube, bar, wire, and more. For detailed chemical composition and free samples, please contact our factory today. We offer competitive pricing and excellent service.

 